Login

MIG PRACTICE

MIG welding practice

More wire feed means more current, and the voltage has to follow. Travel speed sets the leg, gun angle sets how evenly both plates melt. Set the dials, run a bead and cut it open.

Pick a joint

Wire diameter
Wire feed speedCurrent ≈ 53 A3.0 m/min
Voltage28.0 V
Travel speed≈ 48 cm/min8.0 mm/s
Stickout10 mm
Work angleon bisector0 °
Travel anglepush10 °
CO₂ flow15 L/min

Does the voltage match the current?

The green band is the right voltage for this current. More wire feed means more current, so the voltage must follow.

0 A100 A200 A300 A15 V20 V25 V30 V

Bead from above

This 80 mm pass takes 10.0 s
Set it up, then strike an arc
Playback
1× = real time

Technique: straight stringer

The temperature field is solved live from the heat equation (average steel properties); the pool is everything above 1500 °C. Its surface is solved live from surface tension, arc pressure, gravity and metal volume; ripples are the sloshing surface frozen by the solidification front, and oxide islands drift with the surface flow. Illustrative: the score and defects come from the section below.

Your score shows here; the cross-section is below

Cut it open

Set the dials, then strike an arc

A teaching model of how the settings interact. Values are in the range of public procedure charts. Not a qualified procedure: follow your wire maker and your own WPS.

Consumable quantities: Weld & consumable calculator · Daily games